Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ASTM D790 |
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790 |
Network Polymers NPP 30-3500 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D 790 |
Total Finathene® 5302 HDPE drain tile, corrugated pipe resin
(discontinued **) Applications: corrugated pipe, storm and sanitary sewers, drainage systemsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics produc.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.31 - 10.3 GPa | 190 - 1500 ksi | Average value: 4.09 GPa Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790B |
Ineos R35C-00 Polypropylene Random Copolymer Grade R35C-00 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PP1-2002ARX Biocompatible Polypropylene Homopolymer A biocompatible 20 melt injection molding grade of Polypropylene homopolymer for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.31 GPa @Temperature 100 °C |
190 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® ET-1000 HS Polyphthalamide (PPA) (Dry) Amodel® ET-1000 HS is an impact modified, heat stabilized polyphthalamide (PPA) that exhibits exceptional impact strength and toughness. Like all Amodel® PPA resins, ET-1000 HS offers high fat.. |
|||
Flexural Modulus | >= 1.31 GPa | >= 190 ksi | ASTM D790 |
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Formosa Plastics Formolene® HB5202A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5202A is designed for applications requiring excellent stiffness and stress crack resistance propertiesAppl.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 394 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | tangent; ASTM D790 |
Entec Hypro™ PPC-CC10 Natural Copolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem MV-501 Impact Copolymer Polypropylene Description: Long term heat stability, nucleated, excellent processability.Applications: Suggested uses include compounding, thin-walled injection molding.Process: Injection Molding.This resin meets.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI41000WM Impact Copolymer Polypropylene Description: High flexural modulus, excellent mold release, antistatic.Applications: Suggested uses include intricately designed parts, thin-walled parts, dairy containers.Process: Injection Molding.. |
|||
Flexural Modulus | 1.31 - 1.59 GPa | 190 - 230 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 3272 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This high flow resin allows fast injection cycles and provides good impact strength, rigidity, and warpage resistance. This product me.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer
(discontinued **) Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in.. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | ASTM D790 |
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.31 GPa | 190 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AM55-003 Blow Molding Resin
(discontinued **) AM55-003 is a blow molding grade high density polyethylene copolymer containing an excellent antistat additive. It provides a good combination of stiffness and stress crack resistance. AM55-003 co.. |