Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.7 GPa @Temperature 23.0 °C |
1550 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 35 H3.0 000000 Nylon 6, Glass Fiber Reinforced PA 6, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PBT GF30 CF10 FR 30/10% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber, 30/10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF40 L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation p.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PPA GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthInformat.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific) Glass reinforced. Flame retardant. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East) LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM-D790 |
Polyram Polytron A30B02 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 NAT PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer Lehvoss Compounds Luvotech™ J-4/30/V0 RD6922 PA6/12
(discontinued **) Techmer Lehvoss Compounds, a JV between Techmer ES and Lehmann&Voss&Co. has been terminated. |
|||
Flexural Modulus | 10.7 GPa | 1550 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF30 FR HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInform.. |