Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.50 GPa | 1230 ksi | ISO 178 |
Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 8.50 GPa @Temperature 23.0 °C |
1230 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANAMID 66 A12^ F25 NH10 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | |
Lehmann & Voss LUVOCOM® 19-7221/OR Polyamide 46, with glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ISO 178 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 130 CS DUS008 600091 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-G30 30% Glass Fiber Reinforced PA66 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2mm/min; ASTM D790 |
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 2310F PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU2310 PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DE0021E PC LNP STAT-KON* DE0021E is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding, Flame Retardant, Electrically Conductive. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | |
SPS Guang Zhou PONYLâ„¢ EP4003G25 Non-halogen flame retardance/GF25%-PA66 Characteristic: Good flame retardance, high mechanical properties, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DX06094 PC (Europe-Africa-Middle East) LNP* THERMOCOMP* DX06094 is a compound based on Polycarbonate resin containing Glass Fiber . Added features include: High Impact, Non- Brominated & Non-Chlorinated Flame Retardant and Mold Release... |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 226F7 Nylon 6.6, 35% Glass Fiber SAXAMID 226F7 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 35% glass fibers. It has very high mechanical strength in combination with good impact resistance. It is char.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
Plenco 00755 Melamine-Phenolic, Granular, Injection Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM-D790 |
Polyram PlusTek PA360G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced with molybdenum disulfide polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM-D790 |
Polyram RamSter PF300J50 PBT, 50% Glass Fiber + Glass beads 50% Glass-fiber and glass beads reinforced PBT.Information provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
Toyobo VYLOPET® EMC532 Injection Molding Polyester Resin, Glass Reinforced Applications: Auto-partsFeatures: Ultrasonic weldabilityGlass fiber reinforcementInformation provided by Toyobo. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ISO 178 |
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)
(Unverified Data**) 25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio.. |
|||
Flexural Modulus | 8.48 GPa | 1230 ksi | ASTM D790 |
Asahi Kasei Thermofil N-33FG-1626 33% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® 301-G30F PBT Resin 30% glass fiber reinforced, flame retardant, good flow, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
BLUESTAR 403HF-G30 PBT, 30% Glass Filled Typical Applications: Halogen Free; E/E connectors, socketsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East) VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load.. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | |
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Flexural Modulus | 8.50 GPa | 1230 ksi | ASTM D790 |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |