Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 123 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.850 GPa

@Temperature 90.0 °C
123 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilamid A H2 FR HF2 Unfilled, Flame Retardant PA66/6 Co-Polymer
Description: Nilamid A H2 FR HF2 is an unfilled, flame retardant NYLON 66/6 co-polymer that does not contain halogen or red phosphorous. This product combines excellent flow characteristics and extr..
Flexural Modulus >= 0.850 GPa
>= 123 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PE 4441R (40404) Medium Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Flexural Modulus >= 0.850 GPa
>= 123 ksi
ASTM D790
NIZHNEKAMSKNEFTEKHIM PP 4210L (EP2C30F) Propylene and Ethylene Copolymer
Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r..
Flexural Modulus 0.848 GPa
123 ksi
1% Secant; ASTM D790
Ravago Manufacturing Americas Echo® RPPC 20/10 BK Recycled Polypropylene
Copolymer Polypropylene, Unreinforced, 20 MFI, 10 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT,..
Flexural Modulus 0.850 GPa
123 ksi
Secant; ASTM D3350
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin
Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid..
Flexural Modulus 0.850 GPa
123 ksi
Tangent; ASTM D790
Flint Hills AP7710-HS Impact Copolymer Polypropylene
TPO copolymer, UL certified, and FDA compliant.Features: Structural stiffness, ultra high impact strength, and high uniform flow rate.Applications: Injection molding: automotive items and exterior e..
Flexural Modulus 0.850 GPa

@Temperature 23.0 °C
123 ksi

@Temperature 73.4 °F
ISO 178
MBA Polymers PP 2182 Post-consumer recycled polypropylene copolymer
Very high melt flow rate for injection molding application. Available in standard black.Information provided by MBA Polymers.
Flexural Modulus 0.850 GPa
123 ksi
1% Secant; ASTM D790
IRPC Polimaxx Polene 3325M Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD SEALABLE CONTAINS SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM EXTRUSION CPP FILM FOR LAMINATE , CPP FILM FOR PACKAGINGS
Flexural Modulus 0.850 GPa
123 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE
LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated.
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Solvay TECHNYL® C 442 Black V PA6, DRY
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha..
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Borealis Borstar® HE 6068 Natural Bimodal HDPE with very low shrinkage for Submarine and Fiber Optical Cables
Borstar® HE6068 is a natural, UV-stabilized, colorable, bimodal high density (HD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar®..
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790/1
Borealis Borstar® HE6067 Black Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Borstar HE6067 is a black, bimodal, co-polymer high density polyethylene (HDPE) compound produced according to the bimodal Borstar process. It is characterized by its balanced properties important ..
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Borealis Daploy™ WB260HMS Polypropylene
Daploy™ WB260HMS is a propylene-based, structurally isomeric polymer. Applications: cushioning and protective packaging, door liners, lightweight packaging trays, beakers and containers, microwave..
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Flexural Modulus 0.850 GPa
123 ksi
at 2 in/min; ASTM D790
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene
DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman.
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Borealis RD735CF Polypropylene Random Copolymer
RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging ..
Flexural Modulus 0.850 GPa

@Temperature 23.0 °C
123 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® FN727 BK230A Nylon 6
Zytel® FN727 BK230A is a black, impact modified, plasticizer free, very flexible polyamide 6 alloy resin having good low temperature toughness, good heat aging and good chemical resistance. Uses in..
Flexural Modulus 0.850 GPa
123 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® LC6601 BK551 Nylon 612  (Unverified Data**)
Plasticized Toughened Polyamide 612 Developed for Extrusion Information provided by DuPont Performance Polymers
Flexural Modulus 0.850 GPa

@Temperature 23.0 °C
123 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6  (Unverified Data**)
Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an..
Flexural Modulus 0.850 GPa
123 ksi
SAE J949
Azdel SuperLite® SL550900-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL550900-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Carmel Olefins CAPILENE® TU 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® TU 75 AV is a high melt flow rate, controlled rheology heterophasic copolymer with very high impact strength, even at low temperature. It contains antistatic and nucleating..
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
NOVA Chemicals Sclair® 2607-UV9 HDPE Injection Molding Resin  (discontinued **)
Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer.
Flexural Modulus 0.850 GPa
123 ksi
Total Lacqtene® 6002 FLG 42 HDPE film  (discontinued **)
LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h..
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Polyplastic Armlen® PP 3IM Impact Modified Polypropylene
Impact modified polypropylene composite materialInformation provided by PolyPlastic Group.
Flexural Modulus 0.850 GPa
123 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Solvay Engineered Polymers DEXPRO® R120 TPV - High-Impact Polypropylene  (discontinued **)
Description: DEXPRO® R120 is a reactor-grade thermoplastic elastomeric olefin resin with a good balance of impact performance, stiffness, and paintability. Applications: Painted bumper fasciasInfor..
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790/1
Borealis Borstar® HE6062 HDPE Black Jacketing Compound
Borstar HE6062 is a black, bimodal co-polymer high density polyethylene (HDPE) compound produced using the Borealis Borstar process. It is characterized by balanced properties important in jacketin..
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Borealis Borstar® HE6063 Natural Bimodal HD Polyethylene Compound for Jacketing of Communication and Power Cables
Borstar HE6063 is a natural, colorable, bimodal, high-density polyethylene compound, produced using the Borstar process, for jacketing of power and telecommunications cables. It is characterized by..
Copyright © lookpolymers.com All Rights Reserved