Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.759 GPa | 110 ksi | ISO METHOD 178 |
NYCOA 2046 Copolymer Nylon 6/69 extrusion, moderate melt viscosity, high strength mono.Information provided by NYCOA, Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-425 Thermoplastic Polyolefin, UV Stabilized, YBWA Platinum Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% Secant; ASTM D790 |
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excel.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE
(discontinued **) Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa.. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-418N/M358Y Natural medium density ethylene hexene copolymer/yellow concrete
( Benefits: environmentally-friendly pigment system, yellow color for easy identification, outstanding pipe rind ESCR, UV stabilizer in natural resin, concentrate base resinCharacteristics: Pipe Ring .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 0.758 - 13.5 GPa | 110 - 1960 ksi | Average value: 7.83 GPa Grade Count:663 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
BASF Capron® 8224 HSL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.759 GPa | 110 ksi | ASTM D790 |
Flint Hills P5M5R-083 Random Copolymer Polypropylene Features: Radiation resistant. Product does not contain animal derived components. Phthalate-freeApplications: Injection molded parts. Radiation sterilizable medical devices and lab wareInforma.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.759 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP4401 Pipe HDPE High Density Hexene CopolymerApplications: Potable water, industrial mining, oil and gas gatheringsFormolene HP4401 is a high performance copolymer that is designed for the most demanding requiremen.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% secant; ASTM D790 |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | |
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10 Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | |
CMW® ELKONITE® G18 Molybdenum Silver contact material ASTM 662, Class B, infiltrated For arcing electrical contacts especially where low mass is required.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM Test |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Flexural Modulus | 0.760 GPa | 110 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2514 MDPE Injection Molding Resin
(discontinued **) Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Roll-out cart lids, housewares, deep skirt lids,.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Flam™ 1502 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |