Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D785
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Modulus 0.758 GPa
110 ksi
ASTM D790
Izod Impact, Notched 6.75 J/cm
12.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648