Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.14 - 24.1 GPa | 600 - 3500 ksi | Average value: 9.97 GPa Grade Count:52 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Flexural Modulus | 3.80 - 24.1 GPa | 551 - 3500 ksi | Average value: 9.61 GPa Grade Count:155 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Flexural Modulus | 2.00 - 24.1 GPa | 290 - 3500 ksi | Average value: 7.17 GPa Grade Count:230 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 2.60 - 24.1 GPa | 377 - 3500 ksi | Average value: 12.5 GPa Grade Count:29 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Flexural Modulus | 2.41 - 24.1 GPa | 350 - 3500 ksi | Average value: 13.0 GPa Grade Count:18 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |