Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.31 GPa | 1350 ksi | ISO 178 |
PolyOne Nymax™ GF 600 A 33 Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Network Polymers Nylon 66G33L Description: Black NylonInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Custom Resins Vexel™ E20MG35 , 35% Glass/Mica Reinforced PET
(discontinued **) Description: Vexel™ E20MG35 is a 20% glass fiber / 15% mica reinforced PET. Information provided by Custom Resins. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | 73°F; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1035HLHR Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF33 HS L BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF35 HS L 35% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant and Heat Stabilizer Features: Lubricated and Heat StabilizedProcessi.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM L NAT002 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF50 IM2 L 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact Modified and LubricantFeatures: Impact Modified and LubricatedProcessin.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/30/SI/2 Nylon 66, 30% GFR, 2% Silicone Plaslube silicone lubricated nylon 66 grades are cost-effective wear and friction materials with low coefficients of friction. These grades have a potential for noise reduction due to the migratory.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-3/30/TF/13/SI/2 Nylon 6, 30% GFR, 13% PTFE, 2% Silicone Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Techmer ES Plaslube® J-3/30/TF/15 Nylon 6, 30% GFR, 15% PTFE Plaslube glass fiber reinforced polytetrafluoroethylene (PTFE) lubricated nylon 612 grades offer a unique balance of excellent wear and friction performance with good dimensional stability and mecha.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133L (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthForm: PelletsApplications: Automotive under the hoodInformation provided b.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133LUV (Dry) Nylon 66, 33% Glass Fiber Reinforced, Lubricated, UV Stabilized Features: Good chemical resistanceGrease resistantLubricatedOil resistantHigh rigiditySolvent resistantHigh tensile strengthGood UV resistanceForm: PelletsApplications: Automotive under the hoodOutd.. |
|||
Flexural Modulus | 9.31 GPa | 1350 ksi | ASTM D790 |
LNP Thermocomp® IF-1006 Polyamide 6/12 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |