Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, Dry as Molded
&a AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
LATI LAESTRA G/30 30% Glass Fiber Reinforced Syndiotactic Polystyrene (SPS)
(discontinued **) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | |
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified |
|||
Flexural Modulus | 9.10 GPa @Temperature 23.0 °C |
1320 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ420HP PBT (Asia Pacific) Environmentally responsible, low carbon footprint Valox iQ* resin - Valox* iQ420HP resin is made using iQ-PBT resin and 30% glass fiber reinforcement. Valox* iQ420HP may be used for the production.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V9260CS PET (Asia Pacific) Color Stable Glass filled PET |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East) Color Stable Glass filled PET |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RF007ESS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF007ESS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP UF007SXC PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007SXC is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include : Heat Stabilized . |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT LNP THERMOCOMP* WF006 is a compound based on PBT resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific) LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX95523C PC LNP* STAT-KON* DX95523C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX95523C PC (Asia Pacific) LNP* Stat-kon* DX95523C is a compound based on Polycarbonate resin. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Solvay TECHNYL® 2412GM05-D PA66, 38% glass fiber, DRY Description: Polyamid 66, reinforced with 38% of glass fiber and mineral filler, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2412GM05-D is used in all sectors o.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Plenco 4349 Phenolic, Granular, Transfer Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | Longitudinal |
Goodfellow Polyethylene Fiber/Polyethylene composite Information provided by Goodfellow. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ISO 178 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES (Europe-Africa-Middle East) LNP* Thermocomp* JF006E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 9.10 GPa | 1320 ksi | ASTM D790 |
Solvay TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY Description: Polyamid 66, 30% glass fiber reinforce, for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2411GF6 used in all sectors of industry, offering an excellent com.. |