Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.70 GPa | 1260 ksi | |
Plastcom SLOVAMID 66 GF 25 FRG 5 TS PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | |
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | STN EN ISO 178 |
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2mm/min; ASTM D790 |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP BKV 35 XF 901510 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
Solvay TECHNYL® A 218G V33 Black 41N PA66, 33% glass fiber, DRY Description: TECHNYL® A 218G V33 Black 41N is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This pr.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP PFN16 PA 6 LNP* LUBRICOMP* PFN16 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 2% MOS2. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp RFN16SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN16SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Euro.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX203R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East) PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP SH1100A PA12 LNP* Thermocomp* SH1100A is a Nylon 12, High Specificy Gravity compound containing proprietary fillers. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
Polyplastics Duranex® 303RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178-93 |
Wellman Wellamid® GF30-60 XE-WBK Nylon 6, 30% Glass Reinforced, Weatherable All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178-93 |
Wellman Wellamid® MRGF25/15 22H-NBK1/WE-1364 40% Mineral/Glass Reinforced Nylon 66 Description: Mineral/Glass Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
Toyobo Vylopet® EMC317R Glass Reinforced Polyester, Standard Grade Key Feature: UL-94 classApplications: Glossy surface componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, ch.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ASTM D790 |
Ashley Polymers Ashlene® 528L-30LG Nylon 66, 30% Long Glass Fiber Reinforced Long glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provid.. |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Flexural Modulus | 8.70 GPa | 1260 ksi | ISO 178 |
BASF Ultramid® BG40GM45 HS BK 00130 20/25 % Glass/Mineral Filled PA6 (Dry) Description: Ultramid® BG40GM45 HS BK-130 is a pigmented black, heat stabilized, 45 % glass and mineral fiber reinforced polyamide 6 injection molding compound. It possesses a balance of engineerin.. |