Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178/1A |
Radici Raditer® B RVA 300 Polybutylene Terephthalate with 30% Glass fiber Raditer® B RVA is a range of glass fiber reinforced Polybutylene terephthalate blends for injection molding, with excellent dimensional stability, low warpage and good surface aspect.Information pr.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Nilit FRIANYL B63 GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Nilit FRIANYL B63 H-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Hexion Bakelite™ PF 14694 Phenolic Formaldehyde Resin, High Surface Quality
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds.Application areas: Housing parts, heat shields, cookware fittings.Information provided by Bak AGBak AG became a p.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Hexion Bakelite™ 460124 Phenolic Formaldehyde Resin
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | |
Lehmann & Voss LUVOCOM® 50-7154 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | |
Idemitsu Kosan Xarec® EA 522 SPS, 22% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 (Asia Pacific) LNP* Thermocomp* RF00469S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Tipco Tipcofil® AG 600 - 30% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 30% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GF25-66 XE-N 25% Glass Fiber Reinforced, Engineering Grade Nylon 66 Description: Glass Fiber Reinforced, Engineering Grade Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GFT33NO51-NBK2 33% Glass Fiber Reinforced, Impact Modified Nylon 66 Description: Glass Fiber Reinforced, Impact Modified Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GSF25/15-66 22LH-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178-93 |
Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66 Description: Glass Sphere/Fiber Reinforced Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene DescriptionPolyflam® RPP 1133 is a 30% glass filled, flame retardant copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide ACF2 PA66, 10% Carbon Fiber Reinforced, Heat stabilized, Injection Molding Staramide ACF2 is a 10% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
E-Polymers TEKAMID® TA210GR , 33% Glass Fiber Reinforced PA66, DAM 33% Glass Fiber reinforced, Anti EG, Anti HydrolysisInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790, ISO 178 |
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre filled |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RF006K PA66, Glass Fiber Filled, Injection Molded Staramide RF006K is a Radiation Crosslinkable, Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G25 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | dry; ISO 178 |
DSM Stanyl® TW241F5 PA46-GF25 Heat Stabilized, 25% Glass Reinforced |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T.. |
|||
Flexural Modulus | 7.50 GPa | 1090 ksi | ISO 178 |
Hexion Bakelite™ PF 83 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Switch covers, rolls, handle casings.. |