Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ MX5210-0040 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-40G Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
PolyOne Maxxam™ PPR-40G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
NOVA Chemicals Dylark® 238P20 High Performance Glass Filled Styrenic Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KFL36 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, Conditioned Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RX05495 PA 66 LNP LUBRICOMP* RX05495 is a compound based on Nylon 66 resin containing Glass Bead, Graphite, Glass Fiber. Added features of this material include: Easy Molding. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 4211 PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East) LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Asia Pacific) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PPX ZX09022 PPE+PP (Europe-Africa-Middle East) Thermocomp ZX09022 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile mod.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
Toyobo VYLOPET® EMC310 Injection Molding Polyester Resin Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 21% Glass Spray-up Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
Tipco Tipcolene® SEB 300 FR - UL94-V-0 Flame Retardant, 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer 30% Glass Reinforced, Flame Retardant PP HomopolymerApplications: Electrical & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWUVCP 25% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ASTM D790 |
Plenco 2000 Phenolic, Granular, Transfer Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Flexural Modulus | 7.10 GPa | 1030 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1422 LS WH 171 Polyphthalamide (PPA)
(discontinued **) Amodel A-1422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature range, .. |