Mechanical Properties Metric English Comments
Flexural Modulus 6.07 GPa
880 ksi
1.3 mm/min; ASTM D790
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Flexural Modulus 6.07 GPa
880 ksi
Tangent; ASTM D790
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural
Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin  (discontinued **)
SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2..
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Techmer ES Electrablend® ABS CF10 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Modulus 6.07 GPa
880 ksi
ISO 178
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE LubricantFeatures: Good Wear Resistance, Low Extractables, Lubricat..
Flexural Modulus 6.07 GPa
880 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC
LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: ..
Flexural Modulus 6.07 GPa
880 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific)
20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Chase Plastics CP Pryme® N340HSL (COND, 50% RH) Nylon 6 (Utility Grade), 40% Glass Fiber Reinforced, Heat Stabilized, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET
Information provided by A. Schulman.
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Chesterton ARC SD4i High temperature ceramic reinforced erosion resistant coating
Description: An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10-15 mils) per coat..
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Chesterton MRS SD4i Metal Rebuilding System
An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shri..
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Clariant ABS4500G30 ABS, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Flexural Modulus 6.07 GPa
880 ksi
ASTM D790
Asahi Kasei Thermylene® P6-40FM-2371 40% Glass Fiber/Mica Reinforced, Heat Stabilized
Information provided by Asahi Thermofil