Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.96 GPa | 720 ksi | Tangent; ASTM D790 |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Nylene® Naxel™ PC504 20% Glass Reinforced Polycarbonate Description: Naxel™ PC504 is a 20% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | ASTM D790 |
PolyOne Gravi-Tech™ GRV-NP-110-W-NAT Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | Tangent; ASTM D790 |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 4.96 GPa @Temperature 100 °C |
719 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-1116 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1116 HS polyphthalamide (PPA) is a toughened, heat stabilized 16% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Custom Resins Vexel™ E20GF15 , 15% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF15 is a 15% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS (Asia Pacific) LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF13 FR BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Techmer ES HiFill® PBT G/CF30 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES (Asia Pacific) LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | 0.125 in, injection molded, unannealed; ASTM D790 |
Styron EMERGEâ„¢ 4202-8 MFR Polycarbonate EMERGEâ„¢ PC 4202-8 advanced resin is 20% glass reinforced polycarbonate containing mold release for optimal processing. This resin exhibits high modulus and excellent dimensional stability. Ap.. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Chase Plastics CP Pryme® N110L (Dry) Nylon 6, 10% Glass Fiber Reinforced, Lubricated Features: LubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN313L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated, Recycled Content Features: LubricatedRecycled ContentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM C580 |
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm.. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Ecomass® 1050TU96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting balancing and radiation shielding applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA) AlloyGood ToughnessInformation provided by Techn.. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0640 30% Glass Fiber Reinforced, Heat and Copper Information provided by Asahi Thermofil |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-30FG-0860 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GB40 40% Glass Bead Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 4.96 GPa | 720 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF15 FR BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Flexural Modulus | 4.96 GPa | 719 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp JF002E PES LNP THERMOCOMP* JF002E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the America.. |