Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® NN313L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chase Plastics CP Pryme® NN313L (Dry) Nylon 66, 13% Glass Fiber Reinforced, Lubricated, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: LubricatedRecycled ContentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Filler Content 13 %
13 %
Linear Mold Shrinkage, Flow 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength at Break 117 MPa
17000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Flexural Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 4.96 GPa
720 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm
1.00 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 261 °C
501 °F
Deflection Temperature at 1.8 MPa (264 psi) 241 °C
465 °F
Unannealed; ASTM D648