Flexural Modulus 4.13 GPa
599 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific)
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific)
LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubricomp DFI12E PC
LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli..
Flexural Modulus 4.13 GPa
599 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® EH7020 PBT
MINERAL FILLED, METALLIZABLE
Flexural Modulus 4.13 GPa
599 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® EH7020 PBT (Asia Pacific)
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX99620C PC
LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC (Asia Pacific)
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific)
LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding.
Flexural Modulus 4.13 GPa
599 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MF004SU PP
LNP* THERMOCOMP* MF004SU is a compound based on Polypropylene containing 20% Glass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MX95319 PP
LNP* THERMOCOMP* MX95319 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PF002 PA 6
LNP THERMOCOMP* PF002 is a compound based on Nylon 6 resin containing 10% Glass Fiber.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp WFB51 PBT
LNP THERMOCOMP* WFB51 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Glass Fiber. Added features of this material include: Low Warpage.This data was supplied by SABIC-..
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT
LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC
LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MF004S PP
LNP THERMOCOMP* MF004S is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP
LNP* THERMOCOMP* MFB429 is a compound based on Polypropylene resin containing 10% Glass Fiber, 20% Glass Bead. Added features of this material include: Chemically Coupled, Flame Retardant.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP (Asia Pacific)
LNP* Thermocomp* MFB429 is a compound based on Polypropylene resin containing Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
A. Schulman POLYFLAM™ FCB 1236-8555 General Purpose Homopolymer Polypropylene
DescriptionPolyfort® FCB 1236-8555 is a general purpose homopolymer polypropylene filled with 20% glass fiber.Information provided by A. Schulman.
Copyright © lookpolymers.com All Rights Reserved