Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.60 GPa @Temperature 23.0 °C |
522 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® FXE4271L PC (Asia Pacific) Lexan* FXE4271L is a 10% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific) Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL32 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Flexural Modulus | 3.60 - 8.90 GPa | 522 - 1290 ksi | Average value: 6.97 GPa Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2mm/min; ASTM D790 |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
IRPC Polimaxx Polene 2511PCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Flexural Modulus | 3.60 GPa @Thickness 3.20 mm |
522 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Higlass BJ22GC Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, UV-stabilized, chemically coupled, glass fiber-reinforced polypropylene copolymer, moderately high rigidity, high impact strength, excellen.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ BC142/1AC Polypropylene Copolymer Description: Hostacomâ„¢ BC142/1AC conventional melt flow, 3,600 MPa flexural modulus, precolored, mineral-filled polypropylene copolymer has a good balance of stiffness and impact resistance. It.. |
|||
Flexural Modulus | 3.60 GPa @Temperature 80.0 °C |
522 ksi @Temperature 176 °F |
2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 30YK270 PP SABIC® STAMAX 30YK270 is a 30% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Saint-Gobain Meldin® 7003 Isostatically Molded Bearing Grade MoS2 Filled Polyimide Melidin® 7003 is a thermosetting polyimide that includes 15% molybdenum disulfide self-lubricating filler for wear applications that operate in a vacuum or in very dry conditions. Meldin® 700.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2mm/min; ISO 178 |
Teijin Panlite® GN-3410R Improved Mold Release, Glass Fiber Reinforced, Flame Resistant Polycarbonate Resin GF 10% reinforced, flame retardant and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machin.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP PB006SXS PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PB006SXS is a compound based on PA 6 resin containing Glass Bead. Added features include: Heat Stabilized. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ISO 178-93 |
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM-D790 |
Polyram RamOfin PPC364I6 Polypropylene, 30% Mineral and Glass Fiber 30% mineral and glass fiber reinforced, heat resistant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
Covestro Makrolon® SF810 Polycarbonate, Glass Fiber Reinforced Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Structural foam• 10%.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790, ISO 178 |
EPICHEM Epilon PC GF 10 V0 Polycarbonate, 10% Glass Fiber Characteristics: self-extinguishing V0 at 1,6 mm, 10% glass fibre filled |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS BKB085 is a 14% glass reinforced toughened heat stabilized black polyamide 66 resin.Information provided by DuPont Performanc.. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PK005EI2 PA6, Mineral Fiber Filled, Impact Modified Injection Molded Staramide PK005EI2 is an Impact Modified Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T30L1 Talc Reinforced |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Ashley Polymers Ashlene® 525-13G Nylon 66, 13% Glass Reinforced High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Ashley Polymers Ashlene® P1410 Polycarbonate, 10% Glass Reinforced A 10% glass reinforced polycarbonate for increased mechanical strength and thermal properties. P1413: with UV stabilizer.Data provided by the manufacturer |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339T40L Talc Reinforced |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | cond.; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced 20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Flexural Modulus | 3.60 GPa | 522 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32XXP PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL32XXP is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. |