Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.30 GPa | 479 ksi | |
Plastcom SLOVAMID 6/66 FRc 3 TS PA6/66, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural colour. PA 6 + PA 66 alloy for injection moulding with increased flammability resistance, with nonhalogen flame retardant. Excellent.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Polycasa XT PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Flexural Modulus | 3.30 GPa @Temperature 23.0 °C |
479 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF5020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Nilit FRIANYL A63 HS-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | |
Plastcom SLOVAMID 6 GB 30 TS PA6, 30% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Nilit FRIANYL A63 TF-KV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated and 30% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky EG-930 Acrylic, Injection Grade Injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D790 |
Lucky CH-910 Acrylic, Coextrusion Grade Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000F PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be sup.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000FC PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. NSF-51 certified for selected colors. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East) Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ISO 178-93 |
Wellman Wellamid® GF10-66/6-LI6-NBK4 10% Glass Reinforced, Toughened Nylon 66/6 Description: Glass Reinforced, Toughened Nylon 66/6Information provided by Wellman. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | ASTM D 790 |
Cossa Polimeri ESTASTIR GP 1000 Polystyrene Polystyrene crystal, general purposeGood melt flow rate, stiffness, gloss, excellent transparencyInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 3.30 GPa | 479 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East) Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility.. |