Lucky CH-910 Acrylic, Coextrusion Grade

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Extruded
Manufacturer Lucky
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucky CH-910 Acrylic, Coextrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Coextrusion grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring capability.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955-51
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 97
97
ASTM D785
Tensile Strength, Ultimate 74.0 MPa
10700 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Yield Strength 135 MPa
19600 psi
ASTM D790
Flexural Modulus 3.30 GPa
479 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 98.0 °C
208 °F
Deflection Temp; Load not reported; ASTM D648
98.0 °C
208 °F
Heat Distortion Temp
Vicat Softening Point 105 °C
221 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Transmission, Visible 92 %
92 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149