Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.62 GPa | 380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP J1000AE PES LNP* COLORCOMP* J1000AE is an unfilled Polyethersulfone. Added feature of this grade is: Easy Molding. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
I. Stern 108B Utility Black ABS Features:Good processing characteristicsInjection Molding and ExtrusionApplicationsProfilesPicture Frames, Tubes, RodsSpools, ReelsInformation provided by I. Stern & Co. Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® FRPBT200 PBT, Flame Retarded V-0 rated, unfilled PBTAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT LNP* LUBRICOMP* WI001 is a compound based on PBT containing 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU) Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TS15 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Lubricated, Heat Stabilized and Good Wear ResistanceAppearance: BlackInformation provided by TP Composites, .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PSU TL20 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1285 Glass Fiber-Reinforced Copolymer Polypropylene DescriptionPolyfort® FPP1285 is a 20% glass fiber-reinforced copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 2510 Description: Injection Molding Grade, Medium Impact, Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D-790 |
Axiall MP-6510 Rigid PVC, Molding Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA7718 Sheet Extrusion and Blow Molding Resin
(discontinued **) BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstan.. |