Mechanical Properties Metric English Comments
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Maxxam™ DP-8928-2-1000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Asia Pacific)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant
Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided..
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® ML6451 PC
UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time.
Flexural Modulus 2.59 GPa
375 ksi
Tangent; ASTM D790
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
PolyOne Lubri-Tech™ SY-000/10T-2S Natural Polystyrene (PS), PTFE Lubricated  (discontinued **)
Description/Features:High ImpactPTFE LubricatedInformation provided by PolyOne Corporation.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
Firestone C212-15C Nylon 6, Heat Stabilized
Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone
Flexural Modulus 2.59 GPa
376 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific)
LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System.
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Stat-loy AX06484X ABS
LNP* Stat-Loy* AX06484 is a compound based on ABS resin containing mineral filler. Characteristics of this grade is it is extrudeable and static dissipative.This data was supplied by SABIC-IP for t..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS
Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific)
Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in..
Flexural Modulus 2.59 GPa
376 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX500 PPE (Asia Pacific)
Noryl PX500 is an unfilled modified polyphenylene ether resin capable of multiple conversion routes. This resin is designed for lower odor during conversion than many standard modified PPE resins. ..
Flexural Modulus 2.59 GPa
376 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON 9X04323 PPE+PA66 (Asia Pacific)
LNP* Stat-kon* 9X04323 is a compound based on Noryl GTX resin,Added features of this material include: Electrically Conductive.
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Westlake Plastics Pomalux® Acetal Copolymer
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par..
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Westlake Plastics Pomalux® Acetal Copolymer For Medical Applications
Medical grade Pomalux is made from acetal copolymer resin which allows machined products the ability to retain dimensional integrity, maintain stability in water and most chemicals at elevated tempe..
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant
Data provided by Clariant Masterbatches
Flexural Modulus >= 2.59 GPa
>= 375 ksi
ASTM D790
Buckeye Polymers BP RPP 1009 GK Polypropylene, 10% Glass Filled
Product Information: 10% chemically coupled glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stabilit..