Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products FRP300-00 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1493T PC Copolymer Lexan* EXL1493T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance, with mold release. This resin offers excellent low temperature (-3.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PPX-GP3 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Europe-Africa-Middle East) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 15 mm/min; ASTM D790 |
LG Chemical LI-943 ASA Resin
(discontinued **) Heat resistance, Excellent weather resistance, Well balanced mechanical properties, Superior chemical resistance, Good thermal aging stability, Good moldability and processability, Applications incl.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Hyosung Topilene HJ700 PP HJ700 High Isostatic PP HomopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | |
Kraton® G1650 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
|
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | Type I, 5.1 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | Type I, 1.3 mm/min; ASTM D790 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 2.21 GPa @Thickness 6.40 mm |
320 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron MIF-45 ABS Injection Molding Grade High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali |