Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.15 - 2.40 GPa | 312 - 348 ksi | ASTM D790 |
Prodways PLASTCure Model 300 3D Printing Polymer Good mechanical properties.Broad range of dental model applications.Information provided by Genistar. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL6013 PC (Europe-Africa-Middle East) LEXAN EXL6013 is especially developed for applications requiring a high impact performance combined with an improved chemical resistance over standard polycarbonate. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® 9925A PC (Asia Pacific) Lexan 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® ML1665 PC (Asia Pacific) |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2mm/min; ASTM D790 |
Kingfa PA66-R0N Flame Retardant PA66 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesNo bloomingApplications:Injection moldingConnectorsRelay, bobbins, plugsHousehold appliance partsE & E partsIn.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM STM1700 PEI Copolymer Siltem STM1700 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxici.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL N802 PPE+HIPS (Asia Pacific) PPE/PS 80oC V2 FR high flow |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Tipco Tipcolene® ISRH 35 NF - 20% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow 20% Mineral Reinforced, PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D 790 |
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2.6 mm/min; ASTM D790 |
BLUESTAR LXS 110 PPE-PS Typical Applications: Electrical partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ASTM D790 |
Tipco Tipcolene® FPC 30 PPC - 30% Calcium Carbonate Reinforced Polypropylene Copolymer 30% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | ISO 178 |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 2.15 GPa | 312 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |