Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Asia Pacific) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1484T PC Copolymer Lexan* EXL1484T polycarbonate (PC) siloxane copolymer resin is a UV stabilized, enhanced release transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in c.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1232 PC Copolymer (Europe-Africa-Middle East) 18 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 13 mm/min; ASTM D790 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HFD1212 PC Copolymer (Asia Pacific) 18 MFR LEXAN High Flow Ductile Copolymer |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | |
Kraton® G1702 + PPE blend (20/80) Blending KRATON D and G polymers with PPE significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl MX5569 PPE+PS PPE+PS blend. High Heat. Good balance of flow and impact. Offers good aging performance under heat. Typical applications include Automotive Interiors and Lighting.This data was supplied by SABIC-.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | ASTM D790 |
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPS GP 100-1 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | |
Abatron AboCast 8103-16 One Part Epoxy One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak e.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1434T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers extreme low temperature (-40 C) ductility in combination with me.. |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SLX2071T PC Copolymer (Europe-Africa-Middle East) High viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Flexural Modulus | 2.12 GPa | 307 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |