Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.5 GPa | 1520 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers UTTAP QU HT530 GF Nylon, 30% Glass Reinforced Glass reinforced (30 %) - High Temperature Polyamide Alloy, excellent chemical and electrical resistance, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Solvay Specialty Polymers Primef® 5084 30% GF PPS, Lubricated Grade
(discontinued **) Contains PTFE lubricant. Used for injection molding of high performance parts. |
|||
Flexural Modulus | 10.5 GPa @Temperature 23.0 °C |
1520 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Grupo Repol Dinalon® A1S25 G50 PA66 50% Glass Fiber Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | 2 mm/min; ISO 178-A |
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber PA 66, 35% glass fiberInformation provided by LANXESS. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® SAN GF30 Glass Fiber Reinforced |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXC PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC004SXC is a compound based on PA66 resin containing Carbon Fiber. Added features include: Electrically Conductive, Heat Stabilized. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RC004SXS is a compound based on PA 66 resin containing Carbon Fiber. Added features include; Heat Stabilized, Electrically Conductive. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Plenco 1500 Polyester, Granular, Compression Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | dry; ISO 178 |
DSM Stanyl® TS241B3 PA46-CF15 15% Carbon Reinforced, Lubricated |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | DIN 52457 |
CP-Polymer-Technik Wellamid® 6600 CF10 HWCP 10% Carbon Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G35HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSL NC010 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G35HSLR BK420 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin with improved hydrolysis resistance.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
Ascend Performance Materials Vydyne® R535H NT651 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535H NT651 is 35% glass-fiber reinforced PA66 resin. Available in natural, it is heat-stabilized with an electrically neutral heat stabilizer. It is designed specially for electrical appli.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ISO 178 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Beijing Ranger Chem PBT-201-G25 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 640 Nylon 6/12, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | ASTM D790 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Flexural Modulus | 10.5 GPa | 1520 ksi | dry; ISO 178 |
DSM Stanyl® TS200B3 PA46-CF15 15% Carbon Reinforced |
|||
Flexural Modulus | 10.5 GPa @Temperature 90.0 °C |
1520 ksi @Temperature 194 °F |
ASTM D790 |
LATI LARTON G/40 40% Glass Fiber Filled Polyphenylene sulfide (PPS)
(Unverified Data**) Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex.. |