Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Stanyl® TS200B3 PA46-CF15

Category Polymer , Thermoplastic , Nylon , Nylon 46
Manufacturer DSM Engineering Plastics
Trade Name Stanyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Stanyl® TS200B3 PA46-CF15.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% Carbon Reinforced
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
dry; ISO 1183
Moisture Absorption 3.15 %
3.15 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 110 MPa
16000 psi
cond; ISO 527-1/-2
185 MPa
26800 psi
dry; ISO 527-1/-2
Elongation at Break 2.0 %
2.0 %
dry; ISO 527-1/-2
4.0 %
4.0 %
cond; ISO 527-1/-2
Tensile Modulus 13.0 GPa
1890 ksi
dry; ISO 527-1/-2
Flexural Modulus 5.80 GPa
841 ksi
cond; ISO 178
10.5 GPa
1520 ksi
dry; ISO 178
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
13.9 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C
554 °F
dry; ISO 75-1/-2
Users viewing this material also viewed the following: