Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF30 HS UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF/M40 ML2 GY 40% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Molybdenum Disulfide Lubricant and He.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/20 Polycarbonate, 20% Carbon Fiber Reinforced Carbon Fiber Reinforced |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN130GMD2 (DAM) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | Tangent; ASTM D790 |
Applied Composites 8041 Polyester SMC Industry Application: ElectricalProduct Application: Business MachinesDistinct Features: UL 94-VO, Radiant Panel |
|||
Flexural Modulus | 10.3 - 15.2 GPa | 1500 - 2200 ksi | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 685 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.48% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Flexural Modulus | 10.3 - 11.7 GPa | 1500 - 1700 ksi | |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne Nymax™ GF 1800 43 Natural Nylon 612 with 43% Glass Fiber
(discontinued **) Molded Test Bars: Dry as Molded |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |
|||
Flexural Modulus | 10.3 GPa @Temperature 23.0 °C |
1490 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
LATI LARAMID G/30 30% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |