Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne LubriOne™ NI-30CF/15T-2S Polyamide 610 (Nylon 610) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding 43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 10.3 GPa @Temperature 23.0 °C |
1490 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
PolyOne Edgetek® PS-30GF/000 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
PolyOne Edgetek® PK-30GF/000 HT Polyaryletherketone, Glass Filled
(discontinued **) Description/Features:30% Glass FilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-30CF/10T-2S Nylon 6/12, Carbon Fiber Reinforced, PTFE Lubricated
(discontinued **) Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF43 LE BK 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low Ext.. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GB40 BK 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Chem Polymer Chemlon 143 G Nylon 66, 43% Glass Fiber Reinforced A 43% glass fiber reinforced nylon 66 offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 10.3 - 15.2 GPa | 1500 - 2200 ksi | |
Bulk Molding Compounds BMC 304 Automotive Grade Molding Compound BMC 304 is a low profile, automotive grade molding compound that is suitable for Injection, Compression or Transfer molding operations. BMC 304 can be coated using traditional or electrostatic coati.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Flexural Modulus | 10.3 GPa | 1490 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 10.3 GPa | 1500 ksi | ASTM D790 |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |