Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.86 GPa | 270 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.86 GPa @Thickness 3.17 mm |
270 ksi @Thickness 0.125 in |
ASTM D790 |
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Hyosung Topilene J700-1 PP J700-1 Injection Special Purpose GradeApplications:Disposable syringeHouseware applianceCharacteristics:Slip propertyHigh stiffnessFast cycleInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | |
Kraton® G1657 + PA-6,6 blend (12/8/80) Blending KRATON D and G polymers with PA significantly improves the toughness at both room and low temperatures. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific) LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific) LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | secant; ASTM D790 |
Spartech EP5240 Calcium Carbonate Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications inc.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Spartech Royalite R21 ABS General Purpose Sheet Description: General Purpose SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Techmer ES HiFill® PP GB30 30% Glass Beads Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0180 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP YF002 POLYESTER ELASTOMER LNP* THERMOCOMP* YF002 is a compound based on Poyester Elastomer containing 10% Glass Fiber. Added feature of this grade is: High Modulus. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6 E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6011 PPE+PA6 (Asia Pacific) PA6 based unfilled GTX. High impact. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | tangent; chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 9401 Injection Molding Grade, Ultra High Impact Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Flexural Modulus | 1.86 - 3.38 GPa | 270 - 490 ksi | Average value: 2.76 GPa Grade Count:10 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 1.86 GPa | 270 ksi | ASTM D790 |
Samyang Trihip® B300 High Impact Polystyrene, Flame Retardant Dimensional stability, electrical properties and weather resistance are excellent.B300 is the flame retardant grade.Applications: LCD TV Rear Cover - for high flowOffice Machine Housing (O/A, Print.. |
|||
Flexural Modulus | 1.86 GPa @Thickness 6.40 mm |
270 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |