Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products CS30P100-01UV 30% Ceramic Sphere Reinforced Polypropylene, UV Stabilized, Black Applications: Consumer goodsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | Tangent; ASTM D790 |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Petromont 3000 High Density Polyethylene Resin Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D709A |
Dow INSPIRE™ TF2300 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
PTS Trimid® N66-S100L High Impact Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)
(discontinued **) Description/Features:Mica FilledInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Hyosung Topilene HJ740 PP HJ740 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporatio.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 IM HS L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300STL (DAM) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 20% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5143C Homopolymer Polypropylene Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143C is a polypropylene homopolymer designed for sheet and thermoforming applications, which require exceptional clarity. .. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. Calcium Silicate filled. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was se.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Clariant PA131 Nylon 66, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D-790 |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
Flexural Modulus | 1.72 GPa | 250 ksi | ASTM D790 |
Techmer ES Statiblend® PP TM10 BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.. |
|||
Flexural Modulus | 1.72 GPa | 249 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON QD000I PA 6/10 (Asia Pacific) LNP STAT-KON* QD000I is a compound based on Nylon 6/10 resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |