Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.47 GPa | 213 ksi | |
Plastcom SLOVALEN PQ 83 T 20 PP, 20% mineral filling FeaturesModified PP for injection moulding with the content of 20% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | Tangent; 1.3 mm/min; ASTM D790 |
Mytex Polymers AS33LW Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33LW is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and good .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Omni Plastics OmniTuff™ CPP TF20 Copolymer Polypropylene Talc Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP552N Fiber (Staple) Grade Polypropylene Moplen HP552N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552N is a homopolymer selected by customers for use in high speed.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP552R Fiber (Staple/BCF/CF) Grade Polypropylene Moplen HP552R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP552R is a homopolymer typically used by customers in high speed p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP553P Fiber (Staple) Grade Polypropylene Moplen HP553P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP553P is a homopolymer typically used by customers in high speed p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen HP562S Fiber (Spunbond) Grade Polypropylene Moplen HP562S is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562S is a homopolymer particularly suitable f.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
PolyMirae Moplen EP540R Injection Molding Grade Polypropylene Moplen EP540R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540R is a block copolymer particularly suitable for injection.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Homopolymer; Blow Molding, Sheeting & Profile Extrusion ResinCharacteristics: High Stiffness, Good Impact Resistance, Very Low Odor & Taste Transfer, Designated for Uniloy Blowmol.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
LATI LATILUB 82-01M Nylon 12 Base, 1% Molybdenum Disulfide Self Lubricating Plastic
(discontinued **) Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B200 PP B200 Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:StiffnessFormabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene B200P PP B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene HJ340 PP HJ340 Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J842 PP J842 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D760 |
LG Chemical SEETEC H1501 Polypropylene Homopolymer Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D760 |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | |
Shinil Chemical SHINSTRA PP SE3501 Structural Polymer Bumper SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Modulus | 1.47 GPa @Thickness 3.20 mm |
213 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SP 6520 Permanent Antistatic Polystyrene Characteristics No sloughing Fully colorable Meets MIL-PRF-81705D static decay specification Functions even in low humidity levels Processing Injection molding Extrusion & Forming Applications C.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6430BM High Density Polyethylene Blow Molding Key Characteristics:Excellent stiffnessGood processabilityOdorlessSafe for food contactGood printabilityRecommended Applications:Bottles for drinking water, fruit juice, soft drink, milkAutomotive p.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Tipco Tipcolene® FPC 10 PPC - 10% Calcium Carbonate Reinforced Polypropylene Copolymer 10% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | 1% secant, 0.05 in/min.; ASTM D790A |
ExxonMobil PP1105E1 Homopolymer Product Description: High melt flow rate homopolymer. Particularly suitable for general purpose injection molding.Availability: North America Features:Controlled RheologyGeneral PurposeGood Proces.. |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
Braskem H 103 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling; food and cosmetic packing; toys and household; sealed closures. Information provided by Braskem |
|||
Flexural Modulus | 1.47 GPa | 213 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3727 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 3727 is a 24% mineral filled copolymer polypropylene compound.Information provided by A. Schulman. |