LG Chemical SEETEC H1501 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LG Chemical
Trade Name SEETEC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC H1501 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Applications: Housewares, Toys, ClosuresCAS No. 9003-07-0Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 17 g/10 min

@Load 2.16 kg,
Temperature 230 °C
17 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
50mm/min; ASTM D638
Elongation at Break >= 500 %
>= 500 %
50mm/min; ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D760
Izod Impact, Notched 0.294 J/cm

@Temperature 23.0 °C
0.551 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 - 170 °C
266 - 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Vicat Softening Point 153 °C

@Load 1.00 kg
307 °F

@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C
>= 644 °F
Descriptive Properties Value Comments
Autoignition Temperature >350°C