Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PP 1399 Dissipative Thermoplastic Compound PRE-ELEC® PP 1399 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resi.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS002 PP LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific) LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi.. |
|||
Flexural Modulus | >= 1.40 GPa | >= 203 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1500M (X30G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | 1.40 GPa @Temperature 60.0 °C |
203 ksi @Temperature 140 °F |
ASTM D790 |
LATI LATAN 13 Medium Viscosity Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 6523 Polypropylene Homopolymer, General Purpose Key Features: general purpose polypropylene homopolymer resin, stiff, high resistance to solvents, FDA acceptableApplications: automotive, hospital and institutional ware, housewares, general moldin.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 6524 Polypropylene Homopolymer, Heat- and Extraction-Resistant Key Features: heat and extraction-resistant polypropylene homopolymer resin, FDA acceptable, high resistance to solventsApplications: appliances, automotive under-the-hood applicationsMeets FDA requ.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax SB912 Polypropylene Impact Copolymer Key Features: fully formulated polypropylene copolymer resin, homopolymer-like stiffness wit improved impact strength, resist dust and dirt pick-up, excellent strengthApplications: closures, contain.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | |
Kraton® D1102 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ HSBMG265 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMG265 medium high melt flow, 1,400 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent combination of rigidity, .. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
Styron DGF080.00 ESU Polypropylene Overview: 10% glass filled polypropyleneNaturalMedium flowHeat ResistantInformation provided by Styron |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 50% humidity; ISO 178 |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | tangent; ASTM D790 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | At 2 mm/min; ISO 178 |
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 0.05 in/min; ISO 178 |
CTC SunPro® SP 200 TF 3033 Polypropylene Copolymer, 33% Talc Filled SunPro® SP 200 TF 3033 is a 33% talc filled polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Application: VW TL 52660 MD 03Data .. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 2 mm/min, 4 mm; ISO 178 |
Chi Mei Kibiton® PB-5903 SBC High transparency, high toughness, PS Impact modifier |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant; ASTM D790 |
Braskem H 503 Injection Molding Polypropylene Description: H 503 is a low melt flow rate additivated homopolyme used for general purposes. It is designed for injection molding, raffia extrusion, bioriented film and general extrusion. This produ.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334C10L Calcium Reinforced |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ASTM D790 |
Carmel Olefins CAPILENE® E 50 E Polypropylene Homopolymer CAPILENE® E 50 E is a low melt flow rate polypropylene homopolymer intended for extrusion, thermoforming and blow molding featuring very good process ability and melt stability. Products manufactur.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO 178 |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, Conditioned Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |
|||
Flexural Modulus | 1.40 GPa | 203 ksi | ISO Value |
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |