Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin
(discontinued **) Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
Flexural Modulus | 1.17 - 3.59 GPa | 170 - 520 ksi | Average value: 2.79 GPa Grade Count:100 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP700 Polypropylene Copolymer Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive Interior Parts, Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInform.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
M. Holland Company RP700 Polypropylene Copolymer Features: Antistatic, Medium Clarity, Good FlowUses: Household Goods, KitchenwareApprovals: FDA 21 CFR 176.170(c), Table 2, Cond. B, C, D, E, F, G and HProcessing Method: Injection MoldingInformatio.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | |
Kraton® G1650 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790B |
Ineos L24G-00 Polypropylene Impact Copolymer Grade L24G-00 is a high melt flow rate, antistatic high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus. This mat.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Westlake Plastics Ultra Ethylux® HDPE Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding TOTAL Petrochemicals Polypropylene 3847MR offers good processability, excellent clarity, good toughness and good resistance to typical levels of gamma radiation used to sterilize polypropylene.Easy .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D 790 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin Product Description: BA50-120 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Clariant Renol PA2SP0003 Nylon 6, High Gloss Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TR3020C Random Copolymer Polypropylene Description: Clarified, high flexural modulus. Applications: Suggested uses include extrusion, blow molding, thermoforming. Process: Blow Molding. This resin meets the requirements for olefin polym.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TR3020NT Random Copolymer Polypropylene Description: High flexural modulus, very good mold release. Applications: Suggested uses include extrusion, compression molding, thermoforming. Process: Compression Molding. This resin meets the req.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Secant @ 1% strain; ASTM D-790 |
Bapolene® PP5061 Polypropylene, Injection Grade Bapolene PP5061 is a PP Random Copolymer for injection molding. This resin exhibits good clarity and impact properties. This product meets FDA standards for food contact applications.Applications:.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 002-12 RC Clarified Random Copolymer Features:low flowcontainers clarifiersexcellent processingexcellent clarityApplications:bottlescontainersFormer A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |