Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TOTAL Petrochemicals Polypropylene 3847MR offers good processability, excellent clarity, good toughness and good resistance to typical levels of gamma radiation used to sterilize polypropylene.Easy Flow TOTAL Polypropylene 3847MR exhibits exceptionally easy flow characteristics.Recommended Applications. TOTAL Polypropylene 3847MR is recommended for injection molding laboratory and medical applications; however, due to its unique combination of properties, other applications may exist.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 45 g/10 min
45 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256A
Izod Impact, Unnotched NB
NB
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 157 °C
315 °F
DSC
Users viewing this material also viewed the following: