Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
RheTech Products FT3150-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsUnderhood componentsBumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
RheTech Products FT4900-746UV Thermoplastic Polyolefin, UV Stabilized, CD7 Dark Slate Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 2 mm/min; ISO 178 |
Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled AS171L-02US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability.This product is available .. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; ASTM D 790 |
Chevron Phillips HiD® 9354 HDPE Natural Pipe Resin
(discontinued **) Resin Type: gas phase linear hexane copolymerApplications: corrugated pipe applicationsInformation provided by Chevron Phillips Chemical Company. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
Flint Hills AP6412-HS Impact Copolymer Polypropylene High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and .. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer Description: Hostacomâ„¢ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Techmer ES HiFill® PA11 GL8 HS UV Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Graphite Powder Lubricant and UV StabilizerFeatures: Heat Stabilized. Good UV Resistance and LubricatedAppearance: Natural ColorIn.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding Applications:CrateAerosol capsHouse waresInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100HSL (COND, 50% RH) Nylon 66, Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN100L (COND, 50% RH) Nylon 66, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | at 1% secant; ASTM D790 |
A. Schulman SUPERLINEAR™ XL 0370 Rotational Molding Resin DescriptionSuperlinear XL 0370 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 0.05 in.min, tangent; ASTM D790 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 0.05 in.min, tangent; ASTM D790 |
A. Schulman PP 3457-01 Copolymer Polypropylene DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
ExxonMobil HDPE HMA 035 High Density Polyethylene Resin Product Description: HMA 035 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, good impact strength and very high stiffness. Availability: Africa & Middle East, Asia .. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant; ASTM D790 |
Braskem CP 741 Blow Molding Polypropylene Description: CP 741 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and general purpose additive package. CP 741 presents low odor/taste transfer, high mel.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Buckeye Polymers BP Flex D8020 UC85 TPO TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
Polimeri Europa Eraclene® ML 70 High Density Polyethylene - Injection Molding Eraclene ML 70 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Its narrow molecular weight distribution leads to high mechanical properties .. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |
|||
Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |