Material Notes:
Product Description: HMA 035 is a UV stabilized HDPE grade, characterized by excellent dimensional stability, good impact strength and very high stiffness. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: YesUV Stabilizer: YesApplications: Industrial PailsVegetable and Bottle CratesInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.964 g/cc
0.0348 lb/in³
ASTM D4883
ESCR 10% Igepal® 4.0 hour

@Temperature 50.0 °C
4.0 hour

@Temperature 122 °F
F50; ASTM D1963
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
ISO 527-2/1A/50
Elongation at Break >= 100 %
>= 100 %
ISO 527-2/1A/50
Elongation at Yield 9.0 %
9.0 %
ISO 527-2/1A/50
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Izod Impact, Notched (ISO) 6.93 kJ/m²
3.30 ft-lb/in²
ISO 180/1A
Thermal Properties Metric English Comments
Melting Point <= 273 °C
<= 523 °F
Peak Melting Point; ExxonMobil method
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75-2/B