Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Multibase Multi-Pro® 0405 Polypropylene Features: Impact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Nylex™ 1230 Polyamide + PP Forms: PelletsInformation provided by Multibase |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 20-3401 Description: Random Copolymer Polypropylene, ClarifiedInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 20-3401 NC Description: Random Copolymer Polypropylene, Non ClarifiedInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.862 - 1.21 GPa | 125 - 175 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-2000 Description: Utility Grade High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
M. Holland Company CP330 Polypropylene Impact Copolymer AntistaticImpact copolymerMedium flowHigh impact resistanceNucleatedApplications: CratesPailsInformation provided by M. Holland |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Global PCC-0310 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D747 |
Ineos A60-70-162 HDPE Ineos A60-70-162 is a high density polyethylene homopolymer, developed specifically for blow molding food containers on reciprocating screw-type equipment. It exhibits excellent processing character.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790B |
Ineos N20G-00 Polypropylene Impact Copolymer Grade N20G-00 is a high melt flow rate “super-high†impact copolymer polypropylene for injection molding applications. It offers very high impact resistance and good stiffness. This materi.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Lucent Polymers TPO-20T Thermoplastic Polyolefin, 20% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 GF34 IM HS 34% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 34% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned) Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D709A |
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® N200L (COND, 50% RH) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300HSL (COND, 50% RH) Nylon 6 (Utility Grade), Heat Stabilized, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination .. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 3435E Random Copolymer Polypropylene Random Copolymer for Clear Storage Boxes, Pill Vials and Containers Formolene® 3435E is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection mo.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | at 2% Strain; ASTM D3350 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | |
CMW® ELKONITE® 30S Silver Tungsten contact material ASTM B631 For electrical contacts, circuit breakers. Resistant to arcing and welding.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | |
Dow HDPE 17450N High Density Polyethylene DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability ove.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® 4344 HDPE, blow molding
(discontinued **) Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.T.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® PPC100-20M Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® CD 481 HDPE conduit
(discontinued **) Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics product lines. |