Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Multibase Multi-Pro® 0405 Polypropylene Features: Impact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 20-3401 Description: Random Copolymer Polypropylene, ClarifiedInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 2% Secant, 12.7 mm/min; ASTM D790 |
Eastman E6837-539A Polyethylene
(discontinued **) PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® TR-0338-UI Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | 1% Strain Value from rotomolded samples; ASTM D790 |
NOVA Chemicals Novapol® TR-0338-UIG Hexene MDPE Rotational Molding Resin Excellent low temperature impact properties, Excellent ESCR, Good stiffness, Wide processing windowApplications: General purpose custom molding, Chemical containers, IBCs, Fish boxes, Septic tanks, .. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2607 HDPE Injection Molding Resin Features: Excellent stiffness, good impact resistance, low warpage.Applications: Roll-out carts.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Global PCC-0310 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 811 HS L (Conditioned) Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D709A |
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® N200L (COND, 50% RH) Nylon 6, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Chase Plastics CP Pryme® N300L (COND, 50% RH) Nylon 6 (Utility Grade), Internally Lubricant Information provided by Chase Plastics. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total HP 401N Natural HDPE, pipe Applications: Potable water, gas distribution, industrial and mining, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by T.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene Copolymer for Heavy Duty Injection Molded Applications Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination .. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | Tangent - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren.. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | ASTM D790 |
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Mineral Filled, MDI-based 2-Component Liquid System Mineral filler is RRIMGLOS® 10013. 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialSc.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | at 2% Strain; ASTM D3350 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 0.05 in/min; ISO 178 |
CTC X-PRO CTC PP2020 Polypropylene Impact Copolymer X-PRO PP 2020 is an impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D790 |
Entec Hypel® PEHD4/.955 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | |
Dow HDPE 17450N High Density Polyethylene DOW HDPE 17450N resin is a narrow molecular weight distribution copolymer designed to offer low temperature impact strength and gloss with excellent toughness. This resin has good processability ove.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | ASTM D 790 |
Total Finathene® 4344 HDPE, blow molding
(discontinued **) Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.T.. |
|||
Flexural Modulus | 0.862 GPa | 125 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb.. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | ASTM D790A |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | 0.05 in/min, 1x3"; ASTM D790 |
LyondellBasell DEXFLEX® 711 TPO Description: DEXFLEX® 711 is a thermoplastic olefinic elastomer compounded with post-industrial/post-consumer recycled materials. It is designed for use in applications that are (non-color matched.. |
|||
Flexural Modulus | 0.860 GPa | 125 ksi | Tangent; ISO 178 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |