Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Tangent; ASTM D790 |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1.3mm per min; ASTM D790 |
Formosa Plastics Formolene® L63935U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsFormolene L63935U is fully heat and UV stabilized.Meets all requirements of the U.S. Food and Drug Adminis.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Conditioned; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000STHL UV2 Nylon 6/6
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Good Toughness, Lubricated, Heat StabilizedRoHS CompliantAuto Specifications: GM GMP.PA66.074 Color: BlackF.. |
|||
Flexural Modulus | 0.758 - 13.5 GPa | 110 - 1960 ksi | Average value: 7.83 GPa Grade Count:663 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% Secant; ASTM D780 |
LyondellBasell Petrothene® KR92828 High Density Polyethylene ApplicationsPETROTHENE KR 92828 is a high molecular weight, high density polyethylene-based compound designed for use in jacketing, conduit or wire insulation. KR 92828 contains a carbon black cont.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 2% Secant-Method 1; ASTM D790 |
Ineos K44-06-122 HDPE HDPE K44-06-122 is a natural high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It is recognized by the Plastic Pipe Institute as .. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Teknor Apex Telcar® TL EF-6133L2 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CB 3229 Medium Flow, High Impact Copolymer Polypropylene DescriptionPolyfort® CB 3229 is a medium flow, high impact copolymer polypropylene product for injection molding applications.Information provided by A. Schulman. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Chevron Phillips Marlex® HHM TR-418Q MDPE Hexene Copolymer High performance MDPE resin has been formulated for the demanding requirements of pressure pipe applications. Meets ASTM D4976 PE 225. Meets FDA Regulation 177.1520, suitable for food packaging ap.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% secant; ASTM D790 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow DS6D21 Polypropylene Resin DOW DS6D21 is intended for use in cast film processes. It is particularly suited for applications requiring high clarity.Information provided by DowDow Announced Sale of Global Polypropylene Busine.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | |
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10 Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | |
CMW® ELKONITE® 40S Infiltrated Tungsten Silver contact material ASTM B631 For arcing and current carrying electrical contacts.Information provided by CMW Inc. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D3350 |
Formosa Plastics Formolene® HP4000 Pipe HDPE High Density Hexene Copolymer Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop st.. |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | Method I (3 point load), Procedure B); ASTM D790 |
Multibase Multi-Flam™ 1502 PP Black Polypropylene Features:Flame Retardant Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 0.758 GPa | 110 ksi | ASTM D790 |
Formosa Plastics Formolene® HP3902 Pipe HDPE Natural Medium Density Hexene CopolymerApplications: Pipe for gas distribution, oilfield and other industrial pipe, telecommunications conduit.Formolene HP3902 is a high performance copolymer that i.. |