Flexural Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.50 GPa

@Temperature -40.0 °C
508 ksi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.50 GPa

@Temperature 23.0 °C
508 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.50 GPa

@Temperature 80.0 °C
508 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 3.50 GPa

@Temperature -40.0 °C
508 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Copyright © lookpolymers.com All Rights Reserved