Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE. S.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock, Process Aid Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE. Slip 0 ppm. Antiblock.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: slip, antiblock, and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blendedApplications: thick .. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5355 LDPE Industrial Clarity, General Purpose Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Suited for High Speed Converting, Good Impact Strength, Excellent Processability, Good Sealability, Good OpenabilityApplications:Institutional Packaging, Food.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 5455 LDPE Clear, General Purpose Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Clarity, High Gloss, Good Openability, Good Sealability, Suited for High Speed ConvertingApplications:Bakery and Food Products, Rack and Counter Merchand.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman D4008-F Polyethylene
(discontinued **) Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1%; ASTM D882 |
Braskem Flexus® 9210 LLDPE Blown Film Extrusion
(discontinued **) 25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industr.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | 1% Secant; ASTM D882 |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Secant Modulus, MD | 0.220 GPa | 31.9 ksi | ASTM D882 |
Chevron Phillips 6109M LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |