Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.89 MPa | 1000 psi | Lap |
Parker Chomerics CHO-BOND SV713 Conductive Epoxy CHO-BOND® 700 Series Adhesives for Microelectronics Packaging; these pure silver-filled epoxy pastes are designed to meet the demanding requirements of semiconductor and microelectronic packaging. .. |
|||
Shear Strength | >= 6.89 MPa | >= 1000 psi | Lap, Al/Al |
Resin Technology Group TIGA 920H Flexible Silver Conductive 100 parts resin to 115 parts hardener.TIGA 920-H is a flexible, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications that require high flexibil.. |
|||
Shear Strength | >= 6.89 MPa | >= 1000 psi | Cured, lap, Al/Al, at 25°C |
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas.. |
|||
Shear Strength | >= 6.89 MPa | >= 1000 psi | Al to Al |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
Shear Strength | >= 6.89 MPa | >= 1000 psi | Tensile lap, Al to Al, 30 minute cure at 175°F |
Master Bond Supreme 3HT-80 High Strength Epoxy Adhesive Cures at 80°C Description: Master Bond Supreme 3HT-80 is a one component, heat curing epoxy system featuring excellent physical strength properties and toughness with an eye-catching curing temperature of 170-175.. |
|||
Shear Strength | >= 6.89 MPa | >= 1000 psi | Plate Shear (Beam shear for 12.0 pcf products), W Direction, min |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0037 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Rigid PVC; ASTM D1002-64 |
3M Scotch-Weld™ CA8 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3.. |
|||
Shear Strength | 6.89 MPa @Temperature 49.0 °C |
1000 psi @Temperature 120 °F |
Overlap |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 6.89 MPa @Time 1800 sec |
1000 psi @Time 0.500 hour |
Aluminum, Overlap |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, 71°C water soak for 14 days, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, HCl for 14 days, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Isopropyl Alcohol for 14 days, Substrate Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, PC, Substrate Failure |
3M Scotch-Weld™ DP812 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP812 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ DP8405NS Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP8405NS is a high performance, two-part acrylic adhesives that offer excellent shear, peel and impact performance. These toughened adhesives provide improved adh.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Rigid PVC; ASTM D1002-64 |
3M Scotch-Weld™ CA40H Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity version of CA40 and better void filling capabilities.Information provided by 3M |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Rigid PVC; ASTM D1002-64 |
3M Scotch-Weld™ CA7 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ DP810 Tan Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Plywood, Cohesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 6.89 MPa @Temperature 66.0 °C |
1000 psi @Temperature 151 °F |
Overlap, Polyurethane Finish, Adhesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 6.89 MPa @Temperature 82.0 °C, Time 3.46e+6 sec |
1000 psi @Temperature 180 °F, Time 960 hour |
Overlap, Cured for 7 days at 24°C |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 6.89 MPa @Temperature -55.0 °C |
1000 psi @Temperature -67.0 °F |
Steel Overlap; ASTM D1002 |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Shear Strength | 6.89 MPa @Temperature -55.0 °C |
1000 psi @Temperature -67.0 °F |
Steel Overlap; ASTM D1002 |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Abraded Aluminum, Initial |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 6.89 MPa | 1000 psi | Overlap, Fiberglass |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |