Mechanical Properties Metric English Comments
Shear Strength 0.965 MPa
140 psi
ASTM D1002
Arlon Thermabond® R37340X008 Primerless Electronic Adhesive  (discontinued **)
Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas
Shear Strength 0.965 - 20.0 MPa
140 - 2900 psi
Average value: 4.48 MPa Grade Count:31
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Shear Strength 0.965 - 6.05 MPa
140 - 878 psi
Average value: 2.92 MPa Grade Count:35
Overview of materials for Silicone Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma..
Shear Strength 0.965 MPa
140 psi
Plate Shear, L Direction
Hexcel® HexWeb® ACG®-1/2 Honeycomb Aluminum Commercial Grade
HexWeb Aluminum Commercial Grade honeycomb is made from 3000 series aluminum alloy foil. An organic coating is applied to the foil which provides excellent protection against corrosive atmospheres. ..
Shear Strength 0.965 MPa
140 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR III 1/4-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength >= 0.965 MPa
>= 140 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-10 - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.965 MPa
>= 140 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRP/F35 - 3.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP/F35 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRP/F50 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength 0.965 MPa
140 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® HRP/OX - 3/8 - 3.2 Fiberglass/Phenolic Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod..
Shear Strength 0.965 MPa
140 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR III 3/16-5056-.0007 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Strength 0.965 MPa
140 psi
Plate Shear, L Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.001 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb
Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h..
Shear Strength >= 0.965 MPa
>= 140 psi
Plate Shear, W Direction, min
Hexcel® HexWeb® HRH-10/F50 - 4.5 Nonmetallic Flex-Core Honeycomb
Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo..
Shear Strength >= 0.965 MPa
>= 140 psi
Plate Shear, L Direction, min
Hexcel® HexWeb® HRH-327 - 1/8 - 3.2 Fiberglass Reinforced Polyimide Honeycomb
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a..
Shear Strength 0.965 MPa
140 psi
Lap Shear Strength; ASTM D1002
Arlon Thermabond® 99A90X008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier..
Shear Strength 0.965 MPa
140 psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
Shear Strength 0.965 MPa
140 psi
Overlap, Nylon, 50% RH
3M 5200 Marine Adhesive/Sealant Fast Cure
A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals ..
Shear Strength 0.965 MPa

@Temperature 82.0 °C
140 psi

@Temperature 180 °F
Overlap, Etched Aluminum; ASTM D1002
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
Shear Strength 0.965 MPa
140 psi
Lap; ASTM D1002
Arlon Thermabond® 99A90N008 Primerless Electronic Adhesive  (discontinued **)
Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.
Shear Strength >= 0.965 MPa
>= 140 psi
Plate Shear, W Direction, min, preliminary value obtained from limited testing
Hexcel® HexWeb® CFC™-20-1/8-5.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Shear Strength 0.965 MPa
140 psi
Plate Shear, W Direction, typ
Hexcel® HexWeb® CR-PAA™ 1/4-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..