Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® ET-1001 HS Polyphthalamide (PPA) Resin, at 50% RH
(discontinued **) AMODEL ET-1001 HS resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resist.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Custom Resins Duratel™ MF13 Acetal Copolymer
(discontinued **) Description: Duratel™ MF13 is a 13 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | 5 mm/min; ISO 527 |
Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 1095 °C |
8990 psi @Temperature 2003 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 110 °C |
8990 psi @Temperature 230 °F |
ASTM D638 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Adell YS-10 PC Alloy |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Chemlon 253 H Nylon 6, Impact Modified A medium viscosity impact modified, heat stabilized nylon 6 exhibiting improved toughness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 192-N2 Acetal A general purpose, high viscosity, natural.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Chemlon 104 Nylon 66, Medium Impact GP A medium viscosity, impact-modified, lubricated nylon 66 exhibiting improved toughness.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Formax 630 Acetal, High Flow A 30 melt flow index copolymer acetal for use in products requiring extreme demands on processing characteristics but only moderate demands on mechanical performance.Data provided by the manufacture.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D651 |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Tensile Strength, Ultimate | 62.0 - 83.0 MPa | 8990 - 12000 psi | Average value: 77.0 MPa Grade Count:10 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |