| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | ASTM D792 |
| Water Absorption | 0.020 % | 0.020 % | 24 hr immersion; ASTM D570 |
| Linear Mold Shrinkage | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
| Melt Flow | 4.0 - 6.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.0 - 6.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 70 | 70 | ASTM D785 |
| Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
| Elongation at Break | 150 % | 150 % | ASTM D638 |
| Flexural Strength | 77.9 MPa | 11300 psi | ASTM D790 |
| Flexural Modulus | 2.17 GPa | 315 ksi | ASTM D790 |
| Izod Impact, Notched | 7.47 J/cm @Thickness 3.17 mm |
14.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 123 °C | 253 °F | ASTM D648 |