Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
PolyOne Lubri-Tech™ AT-000/08T Acetal - 8% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
IDI Composites M-102 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
LG Chemical Lupoy 1080-70 Polycarbonate Resin Description: LUPOY PC 1080-70 resin is designed for optical media discs applications. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Ch.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | |
Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compressio.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade Durez 118 Black Phenolic is a two-stage, asbestos free, general purpose molding material. It exhibits improved impact strength and resistance to flexural fatigue for demanding automotive, electrica.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Injection Grade Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings whe.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Lubrizol Isoplast® 2510 Engineering Thermoplastic Polyurethane Resin Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Switchgear, HRC FusesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ISO 37 |
Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | DIN 53504 |
Lubrizol ESTANE® 58156 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638/D412 |
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® PB261WO PPO A general purpose flame retardant resin for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa @Temperature 1093 °C |
6960 psi @Temperature 1999 °F |
ASTM E8 |
ATI Allegheny Ludlum 310 Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | Dynamic tensile strength |
Channel Industries 5800 Lead Zirconate Titanate Piezoelectric Characterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most extensively used .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® 727 Nylon 6 A modified nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® 847 Nylon 6, Film Grade A very high impact, low flexural modulus Nylon 6 resin for molding or extrusion. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | XY; ASTM D638 |
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ISO 527B |
Ineos Nova 202W Crystal Polystyrene High Heat Extrusion Grade
(discontinued **) Excellent heat resistance, Superior melt strengthApplications: Foam insulationProperties were determined on injection molded specimens at 23° and 50% RH unless otherwise specified.Information provi.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D651 |
Resinoid 1312 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D651 |
Resinoid 1360 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Tensile Strength, Ultimate | 48.0 - 550 MPa | 6960 - 79800 psi | Average value: 180 MPa Grade Count:56 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ASTM D638 |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |
|||
Tensile Strength, Ultimate | 48.0 MPa | 6960 psi | ATSM D638 |
Ashley Polymers Ashlene® P258 PPO A high flow grade for applications requiring good impact strength and a high heat deflection temperature.Data provided by the manufacturer |