Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® GP60DB Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Type: Estane® GP 60DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tags.Available in EuropeInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ISO 2781
Maximum Moisture Content 0.050
0.050
Melt Flow 5.0 - 20 g/10 min

@Load 8.70 kg,
Temperature 210 °C
5.0 - 20 g/10 min

@Load 19.2 lb,
Temperature 410 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ISO 37
Elongation at Break 540 %
540 %
ISO 37
Tensile Modulus 0.139 GPa
20.2 ksi
ISO 527
50% Modulus 0.0155 GPa
2.25 ksi
ISO 37
100% Modulus 0.0175 GPa
2.54 ksi
ISO 37
300% Modulus 0.0290 GPa
4.21 ksi
ISO 37
Rebound 33 %
33 %
ISO 4662
Tear Strength 143 kN/m
816 pli
with incision; ISO 34B
179 kN/m
1020 pli
without incision; ISO 34B
Abrasion 37
37
mm<sup>3</sup>; ISO 4649
Compression Set 31 %
31 %
70 hrs./22°C; ISO 815
48 %
48 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 135 °C
275 °F
A50; ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Injection
Nozzle Temperature 210 - 220 °C
410 - 428 °F
Injection
Zone 1 200 - 210 °C
392 - 410 °F
Injection
Zone 2 205 - 215 °C
401 - 419 °F
Injection
Zone 3 215 - 225 °C
419 - 437 °F
Injection
Zone 4 215 - 225 °C
419 - 437 °F
Injection
Drying Temperature 105 °C
221 °F
Dry Time 2.00 - 3.00 hour
2.00 - 3.00 hour
Dew Point -30.0 °C
-22.0 °F