Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.2 - 53.0 MPa
5690 - 7690 psi
Average value: 47.9 MPa Grade Count:13
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
Kolon DIAMAT® IH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
DIN 53455; ASTM D638
Kolon KOPEL® KP3372 General Purpose TPE Resin
KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Shinil Chemical SHINCON ABS Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Shinil Chemical SHINSTAT PE Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
SK Chemicals SKYTHANE® 185A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
SK Chemicals SKYTHANE® U0251M Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
SK Chemicals SKYTHANE® UB601 Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
SK Chemicals SKYTHANE® US210 Magnetic Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
Lubrizol Estane® S185A Thermoplastic Polyurethane
Type: Estane® S185A is a Shore 87A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Prov..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Lubrizol Estane® UB601 Thermoplastic Polyurethane
Type: Estane® UB601 resin is a linear, hydroxyl terminated polyurethane polymer designed to be used as a binder for ink formulations. For ink applications, it gives high hardness to coated surface..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
Lubrizol Estane® X-595A-3FR Thermoplastic Polyurethane
Type: Estane® X595A-3FR TPU is a Shore 94A, polyester type thermoplastic polyurethane elastomer.Uses: Film Blowing, Extrusion.Available in AsiaInformation Provided by The Lubrizol Corporation
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D412
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009...
Tensile Strength, Ultimate 39.2 MPa

@Temperature 260 °C
5690 psi

@Temperature 500 °F
ASTM D1708
Daelim H&L Plavis-C CM Conductive Polyimide Bearing
Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad..
Tensile Strength, Ultimate 39.2 MPa

@Temperature 260 °C
5690 psi

@Temperature 500 °F
ASTM D1708
Daelim H&L Plavis-ESD CM Polyimide Bearing
Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D1708
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing
Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po..
Tensile Strength, Ultimate 39.2 MPa

@Temperature 260 °C
5690 psi

@Temperature 500 °F
ASTM D1708
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing
Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi..
Tensile Strength, Ultimate 39.2 MPa
5690 psi
ASTM D638
Samyang Triel® 5700 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5700 is an extrusion grade.Information provided by Samyang.