Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinil Chemical SHINCON ABS Electro Conductive Polymer

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Shinil Chemical
Trade Name SHINCON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINCON ABS Electro Conductive Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's patented conductive filler dispersion technology with variety of engineering polymers and their alloys to impart permanent static dissipative to electrically conductive property to thermoplastics. SHINCON contains multiwall carbon nanotube (MWCNT), carbon black (CB), and carbon fiber (CF) as a conductive filler. SHINCON are used in injection molding, film or sheet extrusion for the applications where the desired level of conductivity and unique mechanical property are important. A wide range of the surface resistaivity is obtained by SHINCON formulations for the parts and devices depending upon customer needs and applications.Feature and BenefitsPermanent electro conductivityMaintain the physical properties of base resinNo particulates (CNT product)Lighter weightRecyclabilityEasy processingImproved surfaceCost effectiveGrade/Application: Pipe CoatingInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Flexural Strength 58.86 MPa
8537 psi
Flexural Modulus 2.26 GPa
327 ksi
Izod Impact, Notched 1.86 J/cm
3.49 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
Processing Properties Metric English Comments
Processing Temperature 230 °C
446 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved